Skip to content

Austenitic

Austentic Fluid Bed Furnace Surface Treatment:
 
 
 
Process
Materials
Advantage

Austenitic Carburising

600°C – 700°C

NH3 / N2 / Hydrocarbon

Typical cycle time 30mins – 3 hours

 

Low Carbon

Low Alloy Steels eg 1020

 

Significantly increased wear resistance
 
Improved fatigue life.
 
Freedom from galling and seizing.
 
Improved corrosion resistance.
 
No significant dimensional change.
 
 
 
Special Advantage
 
 
Short process cycle time e.g. 10-180 mins compared with Qnn Nitriding 12-90 hours.
   
 
 
 
 
 
Effective on all ferrous materials including carbon steels.
   
 
 
 
 
 
A tougher case in comparison with gas nitriding.